Loading ...

poly(3-hexylthiophene):[6,6]-phenyl-C61-butyric acid methyl ester blend film/poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) layer

Based on

1 Articles
2014 Most recent source

Composition

1

poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate)

PEDOT:PSS
Type Complex Compound
Formula
Role layer
2

poly(3-hexylthiophene):[6,6]-phenyl-C61-butyric acid methyl ester blend film

P3HT:PCBM blend film
Type Nano Material
Formula
Role layer

Applications

Area Application Nanomaterial Variant Source
power generation

More information available to subscribers only.

Or, view sample content

Characterization

Method Nanomaterial Variant Source
grazing incidence X-ray and neutron diffraction

More information/entries available to subscribers only.

Or, view sample content

Preparation

Method 1

Type: Physical formation
Source:
Starting materials
  • poly(styrenesulfonate)
  • poly(3,4-ethylenedioxythiophene)
  1. IuUvKS9D87WrQ11Nk7GAL7
Product

poly(3-hexylthiophene):[6,6]-phenyl-C61-butyric acid methyl ester blend film/poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) layer

Thickness: ~ 40 nm

Medium/Support: none

Method 2

Type: Physical formation
Source:
Starting materials
  • poly(styrenesulfonate)
  • poly(3,4-ethylenedioxythiophene)
  1. v4fqsiR7nl7mNEKeILGOoX
Product

poly(3-hexylthiophene):[6,6]-phenyl-C61-butyric acid methyl ester blend film/poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) layer

Thickness: ~ 40 nm

Medium/Support: none

Method 3

Type: Physical formation
Source:
Starting materials
  • poly(styrenesulfonate)
  • poly(3,4-ethylenedioxythiophene)
  1. 1As8GOQrgSrlAQPKV9kQ4V
Product

poly(3-hexylthiophene):[6,6]-phenyl-C61-butyric acid methyl ester blend film/poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) layer

Thickness: ~ 40 nm

Medium/Support: none

Method 4

Type: Physical formation
Source:
Starting materials
  • poly(styrenesulfonate)
  • poly(3,4-ethylenedioxythiophene)
  1. FRR4ndQPI3EGQSWrktOmmj
Product

poly(3-hexylthiophene):[6,6]-phenyl-C61-butyric acid methyl ester blend film/poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) layer

Thickness: ~ 40 nm

Medium/Support: none

References

Full content is available to subscribers only

To view content please choose from the following:

We use cookies to improve your experience with our site. More information

Sign up for a free trial