gold-copper nanostars

Based on

2 Articles
2015 Most recent source

Composition

1

gold-copper alloy

Au-Cu alloy
Type Complex Compound
Formula
Role raw materials

Characterization

Method Nanomaterial Variant Source
scanning electron microscopy

More information/entries available to subscribers only.

Or, view sample content

Preparation

Method 1

Type: Physical formation
Source:
Starting materials
  1. hsV0tfajBom9zM7uDZcr2
  2. mNeQq5MuJcVnqWpGTttiw4ALGKUxGyQdW7QMV
  3. wbI449MK3z93dnxtgVX
Product

gold-copper nanostars

Diameter: ~ 200 nm

Medium: none

Support: Nanopillared silicon

Method 2

Type: Chemical synthesis
Source:
Starting materials
  • copper(II) chloride
  • gold trichloride hydrochloride
  1. 6Qgsuv4v7bkFLwMu
  2. G58tnSTob1PoLo4tULS6bkv7k0eLKg0QWZYl3YGw
  3. JMLi40
Product

gold-copper nanostars

Branch diameter: ~ 50 - ~ 80 nm

Medium/Support: none

Method 3

Type: Chemical synthesis
Source:
Starting materials
  • copper(II) chloride
  • gold trichloride hydrochloride
  1. Llvj0D1DJLUACkPx
  2. WJvxQ48njsFdLsrTNOYtLeip7aoemtWvdNfhu0TV
  3. NgHr5o
Product

gold-copper nanostars

Branch diameter: ~ 50 - ~ 80 nm

Medium/Support: none

References

Full content is available to subscribers only

To view content please choose from the following:

We use cookies to improve your experience with our site. More information

Sign up for a free trial