gold nanoparticle layer

Based on

1 Articles
2014 Most recent source

Composition

Image only illustrates the order and placement of components as described in literature.

1

2-aminoethane-1-thiol

2-mercaptoethylamine β-mercaptoethylamine 2-aminoethane thiol 2-aminoethanethiol mercaptoethylamine decarboxycysteine aminoethanethiol thioethanolamine β-cysteamine cysteamine 2-AET β-MEA MEA Cys AET CYA MPE MA CA
Type Single Compound
Formula HSCH2CH2NH2
Role layer
2

gold nanoparticles

Au nanoparticles gold NP Au NP AuNP GNP
Type Nano Material
Formula
Role layer

Properties

General physical and chemical properties

Property Value Nanomaterial Variant Source
water contact angle

More information available to subscribers only.

Or, view sample content

Characterization

Method Nanomaterial Variant Source
scanning electron microscopy

More information available to subscribers only.

Or, view sample content

Biological effects

Biological system Test details Nanomaterial Variant Source
mouse embryonic stem cells (mESC R1/E)

More information available to subscribers only.

Or, view sample content

Preparation

Method 1

Type: Chemical synthesis
Source:
Starting materials
  1. Keianw6lOWBdBndEHrudh5hMbTBkVhS
Product

gold nanoparticle layer

RMS roughness: 573 nm

Roughness: ~ 433 nm

Medium: none

Support: gold-coated silicon

Method 2

Type: Chemical synthesis
Source:
Starting materials
  1. nvLOpQ9VvR6s1lnzVU1dM1k9zyOFqBo
Product

gold nanoparticle layer

RMS roughness: 392 nm

Roughness: ~ 270 nm

Medium: none

Support: gold-coated silicon

Method 3

Type: Chemical synthesis
Source:
Starting materials
  1. w1v9G4Z5bjVt31VScG9hBWO9tJMFr1Q
Product

gold nanoparticle layer

RMS roughness: 106 nm

Roughness: ~ 58 nm

Medium: none

Support: gold-coated silicon

Method 4

Type: Chemical synthesis
Source:
Starting materials
  1. ZWUr5xnowzXqTUmEJpadRcIrxfO52qj
Product

gold nanoparticle layer

RMS roughness: 1205 nm

Roughness: ~ 969 nm

Medium: none

Support: gold-coated silicon

Method 5

Type: Chemical synthesis
Source:
Starting materials
  1. X56HPBwFRlvVqhDdL2hbHnvleTIPWij
Product

gold nanoparticle layer

RMS roughness: 920 nm

Roughness: ~ 710 nm

Medium: none

Support: gold-coated silicon

References

Full content is available to subscribers only

To view content please choose from the following:

We use cookies to improve your experience with our site. More information

Sign up for a free trial