antimony/tin dioxide thin film

Based on

1 Articles
2014 Most recent source

Composition

Image only illustrates the order and placement of components as described in literature.

1

stannic oxide

stannic oxide tin dioxide tin oxide
Type Single Compound
Formula SnO2
Role layer
2

antimony

Type Single Compound
Formula Sb
Role layer

Properties

General physical and chemical properties

Property Value Nanomaterial Variant Source
electrical resistivity

More information available to subscribers only.

Or, view sample content

Characterization

Method Nanomaterial Variant Source
atomic force microscopy

More information/entries available to subscribers only.

Or, view sample content

Preparation

Method 1

Type: Physical formation
Source:
Starting materials
  1. p421nj9QB
Product

antimony/tin dioxide thin film

RMS roughness: 0.38 nm

Thickness: 4 nm

Thickness: 40 nm

Medium/Support: none

Method 2

Type: Physical formation
Source:
Starting materials
  1. 7D1RVK1C1
Product

antimony/tin dioxide thin film

Thickness: 75 nm

Thickness: 8 nm

Medium/Support: none

Method 3

Type: Physical formation
Source:
Starting materials
  1. Lh4VHhl1j
Product

antimony/tin dioxide thin film

Thickness: 10 nm

Thickness: 40 nm

Medium/Support: none

Method 4

Type: Physical formation
Source:
Starting materials
  1. 8ekqYr6xo
Product

antimony/tin dioxide thin film

Thickness: 40 nm

Thickness: 9 nm

Medium/Support: none

Method 5

Type: Physical formation
Source:
Starting materials
  1. SEDvQQfUs
Product

antimony/tin dioxide thin film

Thickness: 4 nm

Thickness: 75 nm

Medium/Support: none