SnSxSe1-x thin film

Based on

1 Articles
2015 Most recent source

Composition

Image only illustrates the order and placement of components as described in literature.

1

tin sulfoselenide

Type Complex Compound
Formula
Role raw materials

Properties

General physical and chemical properties

Property Value Nanomaterial Variant Source
band gap

More information/entries available to subscribers only.

Or, view sample content

Applications

Area Application Nanomaterial Variant Source
optoelectronics

More information/entries available to subscribers only.

Or, view sample content

Characterization

Method Nanomaterial Variant Source
atomic force microscopy

More information/entries available to subscribers only.

Or, view sample content

Preparation

Method 1

Type: Chemical synthesis
Source:
Starting materials
  • selenous anhydride
  • sodium thiosulfate
  • stannous chloride
  1. 23zmfSLEZFg9WqehnVI1oKyMaZp8EvHooVquFlxg7y4Qp7nx
  2. rkHTqsVg7Btt6DcM
  3. bXLEvktfR5G4GIA7BVPzzPw3pUF
  4. mMKfi5
  5. ZjEtn4jJrJLztIX0cA6sARzT3aR0BQ8Af0DvH9I
  6. UMoLo
  7. XAdNYK
Product

SnSxSe1-x thin film

Crystallite size: 23.7 - 30.4 nm

Roughness: ~ 16.5 nm

Thickness: ~ 1020 nm

Medium/Support: none

Method 2

Type: Chemical synthesis
Source:
Starting materials
  • selenous anhydride
  • sodium thiosulfate
  • stannous chloride
  1. M0TmRCYbieuudTW35ekg87plPRtgbZ1afzkTOfvbyEIMKkcI
  2. M8t9ndToh5ot0x1s
  3. rTpbmpcXdQWaU8XHW2p6XMU6Zhf
  4. R4gE4U
  5. utRjLrt1DDo5dB306spsLIe8zcwlxkQXyjVhCa
  6. JL0yV
  7. 2KUbGd
Product

SnSxSe1-x thin film

Crystallite size: 25.7 - 44.0 nm

Roughness: ~ 17 nm

Thickness: ~ 950 nm

Medium/Support: none

Method 3

Type: Chemical synthesis
Source:
Starting materials
  • sodium thiosulfate
  • selenous anhydride
  • stannous chloride
  1. XYCFy0ksmT6D9cVn7ZQlrm91kloTujWpJijJyOdhwtih3ORt
  2. X36vnnu3Anvb4Jh5
  3. T5HF4gQ2fZgttgNzk57wo0qgWoe
  4. tkorfc
  5. ssXcFf0uj0k5QdG0bFxilFuR8micK0tSayIoqY
  6. ZZDvK
  7. j4H0uW
Product

SnSxSe1-x thin film

Crystallite size: 36.2 - 46.0 nm

Roughness: ~ 19.5 nm

Thickness: ~ 900 nm

Medium/Support: none

Method 4

Type: Chemical synthesis
Source:
Starting materials
  • selenous anhydride
  • sodium thiosulfate
  • stannous chloride
  1. GimDhuoeV1YbNfC7HlYdVx72COLS84zA3isM0WrO2zauou68
  2. TD7klC5t3YHWP6po
  3. APaYxplh4xFuzsiKYnbM8tu6v7K
  4. LddDPp
  5. yAyeJEIN61rdiKTjLuNYuXAPjk96fKNLLeZ2Ej
  6. 1MNmT
  7. Qt8LTP
Product

SnSxSe1-x thin film

Crystallite size: 51.3 - 51.9 nm

Roughness: ~ 21 nm

Thickness: ~ 850 nm

Medium/Support: none

References

Full content is available to subscribers only

To view content please choose from the following:

We use cookies to improve your experience with our site. More information

Sign up for a free trial