Fe nanoparticle (NP)-assembled films prepared by femtosecond-pulsed laser deposition

Based on

2 Articles
2013 Most recent source

Composition

Image only illustrates the order and placement of components as described in literature.

1

iron nanoparticles

Fe nanoparticles iron NP Fe NP
Type Nano Material
Formula
Role raw materials

Properties

General physical and chemical properties

Property Value Nanomaterial Variant Source
coercivity

More information/entries available to subscribers only.

Or, view sample content

Applications

Area Application Nanomaterial Variant Source
data storage

More information available to subscribers only.

Or, view sample content

Characterization

Method Nanomaterial Variant Source
atomic force microscopy

More information/entries available to subscribers only.

Or, view sample content

Preparation

Method 1

Type: Physical formation
Source:
Starting materials
  • iron
  1. XNrFn
  2. OeA0G
Product

Fe nanoparticle (NP)-assembled films prepared by femtosecond-pulsed laser deposition

RMS roughness: 9 nm

Thickness: ~ 22 nm

Medium/Support: none

Method 2

Type: Physical formation
Source:
Starting materials
  • iron
  1. vlcb5
  2. flGf54o
Product

Fe nanoparticle (NP)-assembled films prepared by femtosecond-pulsed laser deposition

RMS roughness: 8 nm

Thickness: ~ 15 nm

Medium/Support: none

Method 3

Type: Physical formation
Source:
Starting materials
  • iron
  1. hkjN0
  2. Voi07L
Product

Fe nanoparticle (NP)-assembled films prepared by femtosecond-pulsed laser deposition

Crystallite size: 13 - 19 nm

RMS roughness: 34 nm

Thickness: ~ 209 nm

Medium/Support: none

Method 4

Type: Physical formation
Source:
Starting materials
  • iron
  1. vJC2D
  2. JdqDo7
Product

Fe nanoparticle (NP)-assembled films prepared by femtosecond-pulsed laser deposition

RMS roughness: 17 nm

Thickness: ~ 85 nm

Medium/Support: none

Method 5

Type: Physical formation
Source:
Starting materials
  • iron
  1. cOz21
  2. oEDVya
Product

Fe nanoparticle (NP)-assembled films prepared by femtosecond-pulsed laser deposition

RMS roughness: 13 nm

Thickness: ~ 43 nm

Medium/Support: none

References

Full content is available to subscribers only

To view content please choose from the following:


Sign up for a free trial