poly(N-isopropylacrylamide-co-allylamine) hydrogel nanoparticle/Au nanoparticle hybrid colloid

Based on

1 Articles
2014 Most recent source

Composition

Image only illustrates the order and placement of components as described in literature.

1

poly(N-isopropylacrylamide-co-allylamine) hydrogel nanoparticles

poly(N-isopropylacrylamide-co-allylamine) hydrogel colloid poly(N-isopropylacrylamide-co-allylamine) hydrogel NP
Type Nano Material
Formula
Role raw materials
2

citrate-stabilized gold nanoparticles

citrate-stabilized Au nanoparticles citrate capped gold nanoparticles citrate capped Au nanoparticles spherical gold nanoparticles citrate-stabilized gold NP citrate-stabilized Au NP citrate-stabilized AuNP citrate capped gold NP citrate capped Au NP citrate capped AuNP gold nanoparticles citrate capped GNP Au nanoparticles gold nanospheres Au NP
Type Nano Material
Formula
Role raw materials

Properties

Applications

Characterization

Method Nanomaterial Variant Source
dynamic light scattering

More information available to subscribers only.

Or, view sample content

Biological effects

Preparation

Method 1

Type: Physical formation
Source:
  1. PyjbSC3O93k9KGA
Product

poly(N-isopropylacrylamide-co-allylamine) hydrogel nanoparticle/Au nanoparticle hybrid colloid

Hydrodynamic diameter: ~ 22 nm

Medium: water

Support: none

Method 2

Type: Physical formation
Source:
Starting materials
  1. Ay7d9axMg2xsOa9IlcRbnP6luDBfp2z0KlO9Rh12J
Product

poly(N-isopropylacrylamide-co-allylamine) hydrogel nanoparticle/Au nanoparticle hybrid colloid

Hydrodynamic diameter: ~ 22 nm

Medium: water

Support: none

References

Full content is available to subscribers only

To view content please choose from the following:

We use cookies to improve your experience with our site. More information

Sign up for a free trial